Structural Distress Diagnostic Wizard
Follow the forensic protocol to identify failure mechanisms and severity.
Simulating tensile stress trajectory & cracking kinematics per fracture mechanics.
Verify whether crack trajectory correlates with shear span (a/d < 2.5) or negative moment inflection before specifying epoxy injection.
Critical Diagonal Shear Cracking
Forensic Failure Mechanism & Root Cause
Principal diagonal tensile stress exceeding concrete tensile strength, often caused by inadequate shear stirrups, shear overload, or increased live loads.
Temporary prop/shore the beam near mid-span. Restrict live loads above immediately.
ACI 318-19 Section 22.5 & ACI 546R-14
EN 1992-1-1 Cl. 6.2 & EN 1504 Principle 4
Mandatory Non-Destructive Testing (NDT) Protocol
- Ultrasonic Pulse Velocity (ASTM C597 / EN 12504-4) to map crack depth and internal void planes
- Electromagnetic Covermeter (Ferroscan) to confirm stirrup spacing and cover depth
Remedial Engineering Specification
High-pressure structural epoxy injection (ASTM C881 Type I/IV Grade 1) followed by external CFRP shear U-wraps anchored into slab.